NIST High Temp. Superconducting Materials (HTS) Database:

NIST Standard Reference Database 62

Last Update to Data Content: 1996

DOI: https://doi.org/10.18434/T4KP8J


Bibliographic Information

Title: Jc measurement
Author(s): Not Available
Publication: STA Project Data Volume: Not Available Issue: Not Available Year: 1991 Page(s): Not Available
Editor(s): Not Available
Publisher: Science and Technology Agency of Japan
Language: Japanese
Notes: STA sheet number: 139
Keywords: Material Specification, Critical Current Density

Materials and Properties

Bi:2223; [Bi-Sr-Ca-Cu-O]
Material Specification for Bi:2223; [Bi-Sr-Ca-Cu-O] Process:
Notes:
Formula: Bi2Sr2Ca2Cu3O10
Informal Name: Bi:2223
Chemical Family: Bi-Sr-Ca-Cu-O
Chemical Class: Oxide
Structure Type:
Manufacturer:
Commercial Name:
Production Date:
Lot Number: BDKBH
Production Form: Disk
Critical Current Density for Bi:2223; [Bi-Sr-Ca-Cu-O]
Critical Current Density (kA/cm2)
0.411
Measurement Method: Resistivity
Test facility: Chyodendo Kenkyu-bu, Yokohama Kenkyu-syo, Fukugawa Denki Kogyo Location: Laboratory 4105, Yokohama Kenkyu-syo Start date: 27-Feb-91 Environment temperature (avg): 22.5 °C Specimen shape: bulk Specimen size: 2.15 mm x 1.30 mm x 19 mm Material of electrode: indium Electrode contact method: ultrasonic soldering Distance between voltage electrodes: 5 mm Lead line: copper Size of lead line: 0.1 mm diameter Temperature control: soaked in liquid N2 Data derivation method: defining the current which induces 1 µV/cm as Ic, calculating Jc from Ic (area of cross section: 2.15 mm x 1.3 mm = 2.80 mm2)

Cautions: Research Data