Tab Page Summary
anhydride, catalyst, oxide
Ozer N., Barreto T., Buyuklimanli T., Lampert C.M.
Sol. Energy Mater. Sol. Cells 36, 433
Overall Energy Resolution (eV):
Calibration:
Au4f7 = 84.00
Charge Reference:
Adventitious carbon
Energy Scale Evaluation:
Reliable, with two-point correction of energy scale
Comment:
The film was prepared by sol-gel method and annealed (T = 423 K, time = 1 h). FAT mode.
Method of Determining Specimen Composition:
Method of Determining Specimen Crystallinity:
X-ray Diffraction
Specimen Temperature (K):
300