Tab Page Summary
bismuth/copper oxide/strontium titanate
Conard T., Sporken R., Ghijsen J., Yu L.M., Caudano R., Seemann R., et al.
Instruction:- Click the column to sort in ascending or descending order.
- Enter a string in the input box in the column header and press the enter to filter the search result in the selected column.
- Click on the hyperlink in the column for more information.
Total Records: 7
mixed Gaussian/Lorentzian
Anode Material:
other source
Overall Energy Resolution (eV):
0.25
Calibration:
FL = Fermi level
Charge Reference:
Conductor
Energy Scale Evaluation:
Reliable (reported energy within 300 eV of a reference energy)
Comment:
4 A Bi/8 A Cu/SrTiO3(100) was oxidized with atomic oxygen. The thickness was measured using a quartz-crystal thickness monitor. Branching ratio = 0.75
Method of Determining Specimen Composition:
Method of Determining Specimen Crystallinity:
Low-energy Electron Diffraction
Specimen Temperature (K):
300