Tab Page Summary
mercury zinc telluride (Hg0.85Zn0.15Te)
chalcogenide, II-VI semiconductor, telluride
Marbeuf A., Ballutaud D., Triboulet R., Dexpert H., Lagarde P., and Marfaing Y.
J. Phys. Chem. Solids 50, 975
Overall Energy Resolution (eV):
Charge Reference:
Valence band minimum
Energy Scale Evaluation:
Reliable (reported energy within 300 eV of a reference energy)
Method of Determining Specimen Composition:
Method of Determining Specimen Crystallinity:
Specimen Temperature (K):
300