Tab Page Summary
nickel zirconium alloy (64-36)
alloy, non-stoichiometric oxide
Walz B., Oelhafen P., Guntherodt H.-J., Baiker A.
Overall Energy Resolution (eV):
Calibration:
Au4f7 = 84.00
Charge Reference:
Conductor
Energy Scale Evaluation:
Reliable (reported energy within 300 eV of a reference energy)
Comment:
Amorphous alloys were prepared by the melt spinning technique and were oxidized by 80 L O2 exposure at 423 K.
Method of Determining Specimen Composition:
Method of Determining Specimen Crystallinity:
Specimen Temperature (K):
300