Reliable, with one-point correction of energy scale
Comment:
An electron flood gun was used for charge compensation. Glasses were prepared by heating dry mixtures of chemicals in alumina crucible at about 1373 K in air for a period of typically 3 hours. The factors 0.02 and 0,98 are weight parts.