Reliable (reported energy within 300 eV of a reference energy)
Comment:
21 A SiO2/n-type P-doped Si(110) wafer with a carrier concentration of ~5E17 cm-3. The substrate was cleaned by Ar+ ion bombardment followed or not annealing (T = 1000 +- 50 K) by the radiation.