Tab Page Summary
bismuth germanium selenium alloy (10-20-70)
alloy, chalcogenide, IV-VI semiconductor, thin film
Kumar S., Kashyap S.C., Chopra K.L.
Overall Energy Resolution (eV):
Calibration:
Au4f7 = 84.00
Charge Reference:
Conductor
Energy Scale Evaluation:
Reliable, with one-point correction of energy scale
Comment:
n-type Bi10Ge20Se70. Bi content was determined by AES and atomic absorption spectrophotometry. FAT mode.
Method of Determining Specimen Composition:
Method of Determining Specimen Crystallinity:
X-ray Diffraction, Transmission Electron Microscopy
Specimen Temperature (K):
300