Reliable, with one-point correction of energy scale
Comment:
6 - 70 A Cr/poly(phenylacetylene). The thin film was prepared by dissolving the polymer in dried high-purity chloroform and spinning the solution onto a polished thin stainless steel plate. The film thickness was measured using a quartz-crystal thickness monitor.