Comment:
Appropriate amounts of Tl2O3, BaO2, Sr2CuO3, La2O3 and CuO powders were mixed and pelletized. The pellets were sintered at 1153 K for 6 h and then furnace cooled to 300 K. The resultant product were reground and pelletized, and these pellets were anneale