Overall Energy Resolution (eV):
Calibration:
Au4f7,Pd3d5 = 84.00,335.12
Charge Reference:
Conductor
Energy Scale Evaluation:
Reliable, with one-point correction of energy scale
Comment:
1.4 L CH3OD were adsorbed onto Pd(111)-(1x1) at 90 K. The substrate was cleaned by cycles of Ar+ ion bombardment (Ep = 600 - 1000 eV, j = 2 microampres cm-2, T = 1050 K), annealing (T = 1200 K) and O2 treatment (p = 1E-5 Pa, T = 1000 K).
Method of Determining Specimen Composition:
X-ray Photoelectron Spectroscopy
Method of Determining Specimen Crystallinity:
Low-energy Electron Diffraction
Specimen Temperature (K):
90