Comment:
The sample was prepared by the reaction of gaseous pyrrole with Cu2+ exchanged chromia-pillared alpha-zirconium phosphate and calcined (T = 673 K). The composition was determined using chemical, thermal and CNH analyses. The intensity ratio of the neutral/charged nitrogen components was 10.10.