Tab Page Summary
(-C*H2CH(OCH2C*H(C*H3)2)-)n
poly(vinyl isobutyl ether)
mixed Gaussian/Lorentzian
Overall Energy Resolution (eV):
Calibration:
Ag3d5 = 368.27
Charge Reference:
Internal hydrocarbon
Energy Scale Evaluation:
Reliable, with one-point correction of energy scale
Comment:
An electron flood gun (Ep = ~1 eV, Ip = 2.3 A) was used for charge compensation.
Method of Determining Specimen Composition:
X-ray Photoelectron Spectroscopy
Method of Determining Specimen Crystallinity:
Specimen Temperature (K):
300