Tab Page Summary
silver phosphite sulfur ((AgPO3)0.80S0.20)
chalcogenide, glass, phosphite
Chowdari B.V.R., Mok K.F., Xie J.M., Gopalakrishnan R.
J. Non-cryst. Solids 160, 73
Overall Energy Resolution (eV):
Charge Reference:
Adventitious carbon
Energy Scale Evaluation:
Reliable, with one-point correction of energy scale
Comment:
Powder samples of AgPO3 were intimately mixed with sulfur and melted (T = 873-963 K, time = 15-45 min). The samples were annealed for 2 h.
Method of Determining Specimen Composition:
Method of Determining Specimen Crystallinity:
X-ray Diffraction
Specimen Temperature (K):
300