Tab Page Summary
    
    
    
        
        
        
            catalyst, oxide, solid solution
 
        
            
                     
            
            
            
            
            
            
            
            
            
            
            
            
            
            
            
            Overall Energy Resolution (eV):
                 
            Calibration:
                Other, Cr2p3 = 574.35
 
            Charge Reference:
                Conductor
 
            Energy Scale Evaluation:
                Reliable, with one-point correction of energy scale
Comment:
                The oxide was prepared by oxidizing the pure metals in oxygen (p = 1E-5 mbar, T = 773 K) in the spectrometer.
 
            
            
            
            Method of Determining Specimen Composition:
                 
            Method of Determining Specimen Crystallinity:
                 
            Specimen Temperature (K):
                300