Overall Energy Resolution (eV):
Charge Reference:
Internal hydrocarbon
Energy Scale Evaluation:
Reliable, with one-point correction of energy scale
Comment:
0.6 A Ag/PET. The PET was cleaned in a series of solvents and dried in a dry N2 atmosphere, and annealed at ~ 363 K for several hours. The thickness was measured using quartz-crystal thickness monitor, XPS and neutron activation analysis. No x-ray-induce
annealed, reacted, reacted film, thick film
Method of Determining Specimen Composition:
X-ray Photoelectron Spectroscopy
Method of Determining Specimen Crystallinity:
Specimen Temperature (K):
293