Tab Page Summary
    
    
    
        
        
        
            anhydride, catalyst, oxide
 
        
            
            
            
            
            
            
            
            
            
            
            
            
            
            
            
            
            Overall Energy Resolution (eV):
                Charge Reference:
                Adventitious carbon
Energy Scale Evaluation:
                Reliable, with one-point correction of energy scale
Comment:
                The oxide was deposited onto SiO2 substrate at temperatures between 648  and 798 K.
Method of Determining Specimen Composition:
                Method of Determining Specimen Crystallinity:
                X-ray Diffraction
Specimen Temperature (K):