Tab Page Summary
palladium/cerium(IV) dioxide/dialuminum(III) trioxide
Shyu I.Z., Otto K., Watkins W.L.H., Graham G.W., Belitz R.K., and Gandhi H.S.
Overall Energy Resolution (eV):
Calibration:
Pd3d5 = 335.12, FL
Charge Reference:
Adventitious carbon
Energy Scale Evaluation:
Reliable, with one-point correction of energy scale
Comment:
4.5 wt % Pd, 18.4 wt % CeO2/Al2O3 was prepared by impregnation of CeO2/Al2O3 with aqueous solution of Pd(NO3)2 and calcination at 1073 K.
Method of Determining Specimen Composition:
Method of Determining Specimen Crystallinity:
Specimen Temperature (K):
300