Tab Page Summary
actinide, non-stoichiometric oxide
Winer K., Colmenares C.A., Smith R.L., Wooten F.
mixed Gaussian/Lorentzian
Overall Energy Resolution (eV):
Calibration:
Au,Cu = 84.00,932.67
Charge Reference:
Conductor
Energy Scale Evaluation:
One-point correction of energy scale
Comment:
70 L D2O/40 L O2/U, polycrystalline. Exposure to D2O was at 85 K.
Method of Determining Specimen Composition:
Method of Determining Specimen Crystallinity:
Specimen Temperature (K):
220