            anhydride, catalyst, double oxide, oxide
 
        
                Grunert W., Spiro E.S., Feldhaus R., Anders K., Antoshin G.V., and Minachev K.M.
 
            
                     
            
            
            
            
            
            
            
            
            
            
            
            
            
            
            
            Overall Energy Resolution (eV):
                Charge Reference:
                Adventitious carbon
Energy Scale Evaluation:
                Reliable, with one-point correction of energy scale
Comment:
                The WO3 was calcined in air at 823 K for 2 hours prior to use. The composition determined by XPS was WO3. FRR mode. Branching ratio = 0.78
Method of Determining Specimen Composition:
                Method of Determining Specimen Crystallinity:
                Specimen Temperature (K):
                293