Tab Page Summary
gold silver tetratelluride
van Triest A., Folkerts W., Haas C.
J. Phys. Cond. Matter 2, 8733
Overall Energy Resolution (eV):
Calibration:
Au4f7 = 84.00
Charge Reference:
Conductor
Energy Scale Evaluation:
Reliable (reported energy within 300 eV of a reference energy)
Comment:
The sample was cleaned by Ar+ ion bombardment and subsequently annealed (T = 373 K, time = 12 h ).
Method of Determining Specimen Composition:
Method of Determining Specimen Crystallinity:
X-ray Diffraction
Specimen Temperature (K):
293