Reliable, with one-point correction of energy scale
Comment:
The alloy was prepared by mixing pure In and Au in weight ratio corresponding to room temperature stable phase followed by melting the mixture with an electron beam in a vacuum. FAT mode. The spectra were recorded at normal emission.