Tab Page Summary
    
    
    
        
        
        
        
            
            
            
            
            
            
            
            
            
            
            
            
            
            
            
            
            Overall Energy Resolution (eV):
                Calibration:
                Pt4f7 = 71.12
Charge Reference:
                Conductor
Energy Scale Evaluation:
                Reliable, with one-point correction of energy scale
Comment:
                CO/Ni(100), saturation coverage. The substrate was cleaned by oxygen treatment and sputtering-annealing cycles.
Method of Determining Specimen Composition:
                Method of Determining Specimen Crystallinity:
                Specimen Temperature (K):
                300