Tab Page Summary
dibismuth diruthenium heptaoxide
catalyst, double oxide, oxide
Shukla A.K., Kannan A.M., Hegde M.S., Gopalakrishnan J.
Overall Energy Resolution (eV):
Calibration:
Au4f7 = 84.00
Charge Reference:
Conductor
Energy Scale Evaluation:
Reliable, with one-point correction of energy scale
Comment:
The sample was prepared by heating a mixture of the respective oxides in air at 1073 K for 12 hours.
Method of Determining Specimen Composition:
Method of Determining Specimen Crystallinity:
X-ray Diffraction
Specimen Temperature (K):
300