Tab Page Summary
    
    
    
        
            silver phosphite sulfur ((AgPO3)0.75S0.25)
 
        
        
            chalcogenide, glass, phosphite
 
        
                Chowdari B.V.R., Mok K.F., Xie J.M., Gopalakrishnan R.
 
            
                J. Non-cryst. Solids 160, 73
 
                     
            
            
            
            
            
            
            
            
            
            
            
            
            
            
            
            Overall Energy Resolution (eV):
                Charge Reference:
                Adventitious carbon
Energy Scale Evaluation:
                Reliable, with one-point correction of energy scale
Comment:
                Powder samples of AgPO3 were intimately mixed with sulfur and melted (T = 873-963 K, time = 15-45 min). The samples were annealed for 2 h.
Method of Determining Specimen Composition:
                Method of Determining Specimen Crystallinity:
                X-ray Diffraction
Specimen Temperature (K):
                300