Tab Page Summary
copper(II) oxide divanadium pentoxide ((CuO)0.30(V2O5)0.70)
double oxide, glass, oxide
Gopalakrishnan R., Chowdari B.V.R., Tan K.L.
Solid State Ionics 53, 1168
Instruction:- Click the column to sort in ascending or descending order.
- Enter a string in the input box in the column header and press the enter to filter the search result in the selected column.
- Click on the hyperlink in the column for more information.
Total Records: 12
Overall Energy Resolution (eV):
Charge Reference:
Adventitious carbon
Energy Scale Evaluation:
Reliable, with one-point correction of energy scale
Comment:
The mixture of reagent grade CuO and V2O5 was dried (T = 373 K) and melted in air (T = 873 K, time = 60 min).
Method of Determining Specimen Composition:
Method of Determining Specimen Crystallinity:
X-ray Diffraction
Specimen Temperature (K):
300