Comment:
                            The thin films were grown by a reactive ion assited deposition onto Si(100) and glass substrates. The sample was cleaned by  Ar+ ion bombardment (Ep = 4 keV, Ip = ~ 5 mA, time = 60 s).  An electron flood gun (Ep = 4 eV) was used for charge compensation.