Overall Energy Resolution (eV):
Charge Reference:
Adventitious carbon
Energy Scale Evaluation:
Reliable, with one-point correction of energy scale
Comment:
Anatase, TiO2(101).The crystal was grown by chemical transport reaction and annealed in O2 (p = 1E5 Pa, T = 873 K, time = 14 h). The total FWHM was 1.1 eV. The spectra were recorded at normal emission and 25 degrees.
annealed, chemical vapor deposition, crystal, insulator, oxygen pressure
Method of Determining Specimen Composition:
X-ray Photoelectron Spectroscopy
Method of Determining Specimen Crystallinity:
Specimen Temperature (K):
300