IUPAC-NIST Solubility Database
NIST Standard Reference Database 106


Glass Ball as Bullet Solubility System: Sulfur dioxide with Poly(dimethylsiloxane) (PDMS) and Poly(vinyltrimethyl silane) (PVTMS)

Components:
   (1) Poly(dimethylsiloxane) (PDMS); ; [9016-00-6]  NIST Chemistry WebBook for detail
   (2) Poly(vinyltrimethyl silane) (PVTMS); ; [25036-32-2]  NIST Chemistry WebBook for detail
   (3) Sulfur dioxide; SO2; [25036-53-7]  NIST Chemistry WebBook for detail

Original Measurements:
   V.V. Volkov, A.K. Bokarev and S.G. Durgaryan, Vysokomol. Soedin. Ser. B 26, 107 (1985).

Variables:
   Temperature = 298 K
   Pressure = 0-0.4 MPa

Prepared By:
   S.M. Shishatski

Experimental Data:   (Subscripts 1,2,3, ..., in column headings refer to components 1,2,3, ...)
   View Figure 1 for this Evaluation

View Figure 2 for this Evaluation

Method/Apparatus/Procedure:
   Sorption was measured by means of a McBain balance using the technique described in Ref. 1.

Source and Purity of Materials:
   PVTMS: MMn=200 000. PDMS: Mn=150 000. Silane-siloxane block-copolymers of the A-B type: prepared by anionic polymerization; M,(silane block) 200 000, weight contents of siloxane block indicated in Pig. 29.

Estimated Errors:

   Temperature: No information given.

References:
   1V V. Volkov, A. K. Bokarev, and S. G. Durgaryan, Vysokomol, Soedin., Ser. A. 26, 1294 (1984).